W0400 |
|
- Copper Thickness: 0.1mm
- Width: 18mm
- Insulation: 0.125mm PET Plastic
- Temperature Rating: 100°C
- Resistance: 2 Ohms per 100m.
- Roll Length: 50m
|
|
A flat copper tape for building hearing loops encapsulated in a clear PET insulation. Can be folded to run around corners. |
|
W2510 ROHS
|
|
- 1.27mm Pitch.
- Conductors 10 x 0.12mm.
- 30m Roll
|
|
1.27mm Pitch.
Conductors 10 x 0.12mm.
30m Roll |
|
W2610 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 10 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
10 Way. Grey insulation. |
|
W2616 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 16 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
16 Way. Grey insulation. |
|
W2620 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 20 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
20 Way. Grey insulation. |
|
W2524 ROHS
|
|
- 1.27mm Pitch.
- Conductors 10 x 0.12mm.
- 30m Roll
|
|
1.27mm Pitch.
Conductors 10 x 0.12mm.
30m Roll |
|
W2516 ROHS
|
|
- 1.27mm Pitch.
- Conductors 10 x 0.12mm.
- 30m Roll
|
|
1.27mm Pitch.
Conductors 10 x 0.12mm.
30m Roll |
|
W2640 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 40 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
40 Way. Grey insulation. |
|
W2614 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 14 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
14 Way. Grey insulation. |
|
W2626 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 26 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
26 Way, 1.27mm pitch. Grey insulation. |
|
W2650 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 50 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
50 Way. Grey insulation. |
|
W2634 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 34 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
34 Way. Grey insulation. |
|
W2625 ROHS
|
|
- Conductor
- Size: 28AWG (0.89mm2)
- Material: tinned copper
- Construction: 7/0.127mm
- Insulation
- Material: Fire resistant PVC 105ºC
- Average thickness: 0.26mm
- Minimum thickness: 0.18mm
- Diameter: 20 x 1.29±0.15mm
- Colour: grey (edge with red trace)
- Electric
- Conductor resistance: max. 237Ω/km, 20ºC
- Insulation resistance: min. 100MΩ/km, 20ºC
- Capacitance: 60pF/m (G-S-G), 42pF/m (G-S)
- Inductance: 1.45µH/m
- Impedance: 100±10Ω (G-S-G)
- Propagation delay time 5.0ns/m
- Spark test 2500V
- Dielectric strength: min. 2kV in 1 minute
- Rating voltage: max. 300V
- Rating temperature: -20ºC to 105ºC
- Standard: UL2651/CSA C22.2 No. 210.2
|
|
25 Way. Grey insulation. |